Tehran University of Medical Sciences

Science Communicator Platform

Stay connected! Follow us on X network (Twitter):
Share this content! On (X network) By
Effect of Preparation Design on Marginal Adaptation and Fracture Strength of Ceramic Occlusal Veneers: A Systematic Review Publisher Pubmed



Sirous S1 ; Navadeh A2 ; Ebrahimgol S3 ; Atri F4
Authors
Show Affiliations
Authors Affiliations
  1. 1. Departement of Prosthodontics, School of Dentistry, Islamic Azad University (Khorasgan Branch), Isfahan, Iran
  2. 2. Private Practice, Dubai, United Arab Emirates
  3. 3. Department of Prosthodontics, School of Dentistry, Tehran University of Medical Sciences, Tehran, Iran
  4. 4. Department of Prosthodontics, Dental Research Center, Dentistry Research Institute, Tehran University of Medical Sciences, Tehran, Iran

Source: Clinical and Experimental Dental Research Published:2022


Abstract

Objectives: This systematic review aims to investigate the effect of different preparation designs on the marginal fit and fracture strength of ceramic occlusal veneers. Materials and Methods: Based on the PICO question and the search terms, an electronic search was performed in Google Scholar, PubMed (MEDLINE), Scopus, Cochrane Library, Web of Science, Science Direct, Wiley, Ovid, and SAGE for articles published up to July 2022. After including English in vitro studies that evaluated posterior ceramic occlusal overlays at the posterior with ceramic restorations by following the PRISMA statement, the extracted data was tabulated. The methodological quality of the included studies was evaluated. Risk of bias assessment was done independently by two authors using the modified MINORS scale. Results: About 3138 search results were screened, of which 22 were selected due to their titles. Twenty-one full-text articles were assessed for eligibility. Seventeen in-vitro studies were finalized for the extraction of quantitative data. All 17 articles had a low risk of bias and were retained. The influencing items for evaluating the research were different in most studies; therefore, qualitative synthesis of the results was feasible. They generally included preparation design, material thickness, depth of preparation in the tooth, internal divergence angle, and finish line. Meta-analysis was not done due to heterogeneity of preparation types and evaluation methods. Results revealed that fracture resistance of occlusal veneers is higher than normal mastication force, and it is sufficient to prepare the occlusal surface, use a self-etching primer for bonding, and an acceptable minimum ceramic thickness. The marginal discrepancy of occlusal veneers is clinically acceptable. However, this systematic review faces some limitations due to the lack of in vivo studies, different preparation designs in included studies, different follow-ups, and lack of comprehensive explanations in articles. Conclusions: The preparation design of occlusal veneers influences both marginal adaptation and fracture resistance. Various preparation designs are proven to have clinically acceptable fracture strength and marginal adaptation. © 2022 The Authors. Clinical and Experimental Dental Research published by John Wiley & Sons Ltd.